Skip to search boxSkip to navigationSkip to main content

Microhardness homogeneity of RBCS light-cured with a multiple-peak led and surface characterization after wear

  • Beatriz Ometto Sahadi
    ,
  • ,
  • Carolina Bosso André(corresponding author)
    ,
  • Maicon Sebold
    ,
  • Regina Guenka Palma-Dibb
    ,
  • Juliana Jendiroba Faraoni
*Corresponding author for this work
  • University of Campinas
    ,
  • Universidade Federal de Minas Gerais
    ,
  • University of São Paulo
Research Output:
Contribution to journal
Article
Peer-review

Open access

Publication Information

Output type

Research Output:
Contribution to journal
Article
Peer-review

Original language

English

Pages from-to (Number of pages)

Pages 92-104 (13 pages)

Journal (Volume, Issue Number)

Brazilian Dental Journal (Volume 32, Issue 3)

Publication milestones

  • Published - 2021

Publication status

Published - 2021

ISSN

0103-6440

Publication IDs

  • Scopus: 85120339763

Abstract

This in vitro study evaluated the effect of the beam homogeneity of a multiple-peak light-curing unit on the surface microhardness and the effect of toothbrushing wear on the microhardness, surface roughness, roughness profile, volume loss, and gloss retention of incremental and bulk-fill resin-based composites (RBCs). A LED light-curing unit (VALO) with four LEDs at the tip end (405, 445, 465A, and 465B nm emission peak) was used according to each manufacturer-recommended time to obtain disks (n=10) of six RBCs: Estelite Sigma Quick, Charisma Classic, Tetric EvoCeram Bulk Fill, Filtek Z250, Filtek Supreme Ultra, and Filtek Bulk Fill. Microhardness values were obtained according to each LED positioning of the light-curing unit on the top surface of the RBCs and were analyzed before and after toothbrushing regarding microhardness, surface roughness, roughness profile, volume loss, and gloss retention. Microhardness was considered homogeneous on the top surface regardless of the type of RBC or wavelength tested (p>0.05). Overall, toothbrushing did not reduce the microhardness of the RBCs but influenced the gloss values for most RBCs (p<0.001). Charisma Classic presented the greatest surface roughness and roughness profile after toothbrushing (p<0.05). Volume loss did not differ among RBCs (p>0.05). In conclusion, different wavelengths of the LED did not affect the top surface microhardness, regardless of the RBCs tested; and bulk-fill composites presented similar surface changes (microhardness, surface roughness, roughness profile, volume loss, and gloss retention) when compared to conventional composites after toothbrushing.

Publication metrics

Metrics

Scopus
Citations

PlumX, opens in new tab

Citations
4
Usage
23
Captures
6